产品名称 > 热固油墨系列

发布日期:2016-01-09堆高油墨(拉浆油墨)
名称: 堆高油墨(拉浆油墨)
编号: FH
规格: 20KG、桶
产品类别:热固油墨系列
适用于:服装鞋帽纺织印花
价格:
生产厂家:幸运印花材料有限公司
Product name Plastisol ink with special effect      
State Paste 
Packing 25KG/drum for white, 20KG/drum for other colors
Storage 12 months in cool place
Application 1. Suitable for automatic, manual printing, can create 3D sharp up and round up effects etc.
2. Suitable for all fabrics which endurable in high temperature of 150-180 degree.
Features 1. High fastness
2. High glossy
3. High softness
4. SGS detecting passed, no phthalate, no heavy metal, no NPEOs.
Mix proportion Plastisol ink 100%, or can be intermixed with other colored plastisol inks
Printing process 1. Printing with plastisol ink  for 3-4 times(3-4 scrapes per time)
2. Thin the plastisol ink with thinner before last printing
3. Take up the screen plate slowly and slightly to make the special effect
4. Baking for 1~3 minutes under 150~180℃ to dry it.
5. Finish.
Attentions 1. The fabric must endurable in hot temperature, it’s not suitable for airtight fabric.
2. Thick screen is suggested for the best effect .
3. Please thin the plastisol ink before last printing to make the best effect
品名 热固油墨拉浆                 
外观 糊状
包装 白色25KG/桶,其他色20KG/桶
贮存期 常温下12个月
应用 100%棉、棉/涤混纺、涤纶、深浅色布、牛仔布等各种织物,凡满足以下两点的织物均可使用:
1. 能耐150C~180C;
2. 有透气性,可以使油墨渗透进去。不适合的承印物比如:塑料、金属、玻璃等及经防水处理的尼龙布。
卖点 1. 超强洗水牢度
2. 高亮度
3. 手感柔软
4. 符合美国ASTM对邻苯二甲酸脂和欧盟EN71 Part 3对重金属含量的要求
调配比例 可以直接印花,或用不同颜色相互调配成其他色
工艺流程 1. 丝网选用100-120目厚板,用丝印硬方刀75度刮印2次,印第一次时用力刮4-6刀
2. 最后一次刮印前将热固油墨稍加开稀,印后轻轻起板留浆即可做出拉浆效果
3. 用热风枪吹至表干,然后150-180度焙烘过热1-3分钟,不能压烫
注意事项 1. 最后一次刮印前一定要将油墨开稀,否则无法形成完美的拉浆效果
2. 墨层一定要烘熟,否则会影响牢固度  
                  


分享到